About half the time recently when printing with PLA, I see that holes or loops have a line of filament running approximately through the middle which seems to be one of the inner perimeters having detached and contracted, but is still attached on both sides. Is it a temperature thing, an extrusion thing? I can't find a pattern. Bed adhesion is great. Bambu H2C, mostly printing with Bambu Basic PLA.

you are viewing a single comment's thread
view the rest of the comments
[–] 1 point 5 months ago (1 child)

It looks like that's your first layer? Poor bed adhesion coupled with a slight under extrusion might be doing it. You could also try to slow down your first layer dramatically (50% or more slower)

  • source
  • hideshow 2 child comments
  • [–] [S] 1 point 5 months ago (2 children)

    It's both first layers and higher. No pattern I can find. Bed adhesion is definitely fine, I haven't had a single lifted corner since I started using the SuperTac plate.

  • source
  • parent
  • hideshow 4 child comments
  • [–] 1 point 5 months ago

    I would try bumping the flow up manually a bit, and setting it to run slower. Try changing your filament to Generic in the profile too, if it'll let you.

    Then see if you get a few clean layers trying all of this.

  • source
  • parent