This was an ornament I printed roughly 6 years ago. Being a Christmas ornament it spent most of those 6 years stored in my roof space.

Being in Australia this would have been subject to average temperatures of 30 to 35 degrees c but also peaks across summer approaching 70 degrees c. Also in high humidity.

The PLA crumbles into tiny pieces at the softest touch.

I thought it was interesting that PLA would start to break down in these conditions.

you are viewing a single comment's thread
view the rest of the comments
[–] 21 points 2 years ago*

Not entirely true as there are no industry standards for PLA. Lots of manufacturers add things they don't put on the label. Especially in the variants like PLA+ and High Speed PLA.